Thermal Properties Metric English Comments
Thermal Conductivity 28.0 W/m-K

@Temperature 85.0 °C
194 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy
Higher tensile strength solder than #121. Particular application is joining copper tubing in refrigeration and potable water systems. Has good wettability with good long time sheer strength at 100Â..
Thermal Conductivity 28.0 W/m-K
194 BTU-in/hr-ft²-°F
Parallel to pressing direction
Momentive Performance Materials HBC Hot-Pressed Boron Nitride
Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom..
Thermal Conductivity 28.0 W/m-K
194 BTU-in/hr-ft²-°F
DIN EN 821-2 / ASTM-C408
CeramTec Rubalit® 710 Alumina, 99.6%
Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct..
Thermal Conductivity 28.0 W/m-K
194 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS217 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 28.0 W/m-K
194 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS226A Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 28.0 W/m-K
194 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS238A Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 28.0 W/m-K
194 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS240 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 28.0 W/m-K
194 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS487 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 28.0 W/m-K
194 BTU-in/hr-ft²-°F
Goodfellow Awa®, Nickeloid®, Simlet®, Spedex® Nickel Silver
Good machinability, excellent cold working and welding characteristics. Poor hot forming. Uses include rivets, screws, zippers, optical parts and costume jewelry.Information provided by Goodfello..
Thermal Conductivity 28.0 W/m-K

@Temperature 399 °C
194 BTU-in/hr-ft²-°F

@Temperature 750 °F
hardened and tempered
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel
Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications wh..
Thermal Conductivity 28.0 W/m-K
194 BTU-in/hr-ft²-°F
DIN EN 821-2
CeramTec B 40 Alumina, 99.1%
B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability.