Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | Mean T=20°C; ISO 8301:1991 |
Nylacast POM C Acetal Copolymer The copolymer grade is the ideal combination of strength, stiffness and wears resistance. It absorbs very little moisture, is easily machinable and is genuinely porosity-free making it the preferred.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4-230NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compare.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV31 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV41 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV8262 Red General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV88 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon POM C Polyacetal C Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV560 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV60 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV60 Silicone Rubber Compound for High Temperature, Red RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM UF5011S PEI Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ambient; DIN 52612 |
Brandenburger BL 70 Slide Bearing Material BL 70 is a low friction material that exhibits stability at high temperatures. Its applications include high-load low friction tracks and linings in transport and conveying systems, high-stressed b.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612-1 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
CENTROPLAST CENTROGUARD Polyoxymethylene, Antimicrobial During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micr.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Conditioned) Ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV630 Blue General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |