Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 32.0 W/m-K | 222 BTU-in/hr-ft²-°F | |
Arlon 99410R015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate Design/Construction:Interleave: 0.001" FEPSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and sho.. |