Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 235 W/m-K | 1630 BTU-in/hr-ft²-°F | greater than pure W |
Plansee W-20Cu Tungsten-Copper Composite This composite material is composed of a porous tungsten matrix which is infiltrated with copper.Characteristics:Very resistant to arc erosionGood electrical conductivityHigh thermal conductivityLow.. |