Plansee W-20Cu Tungsten-Copper Composite

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer Plansee SE
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plansee W-20Cu Tungsten-Copper Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This composite material is composed of a porous tungsten matrix which is infiltrated with copper.Characteristics:Very resistant to arc erosionGood electrical conductivityHigh thermal conductivityLow thermal expansion.Typical Applications:High-voltage circuit breakersErosion electrodesRadar technology - base plates and heat spreadersOpto electronicsHigh frequency electronicsInformation provided by Plansee.
Physical Properties Metric English Comments
Specific Gravity 15.5 g/cc
15.5 g/cc
Thermal Properties Metric English Comments
CTE, linear 8.30 µm/m-°C
4.61 µin/in-°F
Thermal Conductivity 235 W/m-K
1630 BTU-in/hr-ft²-°F
greater than pure W
Component Elements Properties Metric English Comments
Copper, Cu 20 %
20 %
Tungsten, W 80 %
80 %
Descriptive Properties Value Comments
Ductility much greater than pure W
Machinability/Workability much greater than pure W