Thermal Properties Metric English Comments
Thermal Conductivity 24.2 W/m-K

@Temperature 800 °C
168 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 24.2 W/m-K

@Temperature 800 °C
168 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 24.2 W/m-K

@Temperature 800 °C
168 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 24.2 W/m-K

@Temperature 800 °C
168 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 24.2 W/m-K

@Temperature 800 °C
168 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 24.2 W/m-K

@Temperature 800 °C
168 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 24.2 W/m-K

@Temperature 800 °C
168 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 24.2 W/m-K

@Temperature 800 °C
168 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 24.2 W/m-K

@Temperature 800 °C
168 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 24.2 W/m-K

@Temperature 392 °C
168 BTU-in/hr-ft²-°F

@Temperature 738 °F
Latrobe 14-4CrMo Stainless Tool Steel
14-4CrMo is a wear resistant, martensitic stainless tool steel that exhibits better corrosion resistance than Type 440C stainless steel. The molybdenum in the steel provides superior corrosion resis..
Thermal Conductivity 24.2 W/m-K
168 BTU-in/hr-ft²-°F
SGL Carbon Group EK 40 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Thermal Conductivity 24.2 W/m-K

@Temperature 95.0 °C
168 BTU-in/hr-ft²-°F

@Temperature 203 °F
Crucible Steel 154 CM Martensitic Steel
Crucible 154 CM is a modification of 440C martensitic stainless steel to which molybdenum has been added. 154 CM has better corrosion resistance, better wear resistance and better hot-hardness than ..
Thermal Conductivity 24.2 W/m-K

@Temperature 93.3 °C
168 BTU-in/hr-ft²-°F

@Temperature 200 °F
Crucible Steel 440A Chromium Steel
Crucible 440A is a hardenable chromium steel which is the toughest of the high chromium cutlery grades. This grade is magnetic at all times. Information provided by Crucible Specialty Metals.
Thermal Conductivity 24.2 W/m-K

@Temperature 93.3 °C
168 BTU-in/hr-ft²-°F

@Temperature 200 °F
Crucible Steel 440B Chromium Steel
Crucible 440B Is a hardenable chromium steel which is cutlery grade having high attainable hardness and toughness. This grade is magnetic at all times. Information provided by Crucible Specialty Me..
Thermal Conductivity 24.2 W/m-K

@Temperature 200 °C
168 BTU-in/hr-ft²-°F

@Temperature 392 °F
Crucible Steel CPM® 3V® Tool Steel
CPM 3V is a new tool steel made by the Crucible Particle Metallurgy process, designed to provide maximum resistance to breakage and chipping in a highly wear-resistant steel. CPM 3V offers impact to..
Thermal Conductivity 24.2 W/m-K
168 BTU-in/hr-ft²-°F
Dura-Bar 80-55-06 Continuously Cast Ductile Iron Bar Stock ASTM A536
Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for..
Thermal Conductivity 24.2 W/m-K

@Temperature 100 °C
168 BTU-in/hr-ft²-°F

@Temperature 212 °F
ATI Allegheny Ludlum 420 Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
Thermal Conductivity 24.2 W/m-K

@Temperature 100 °C
168 BTU-in/hr-ft²-°F

@Temperature 212 °F
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
Thermal Conductivity 24.2 W/m-K

@Temperature 100 °C
168 BTU-in/hr-ft²-°F

@Temperature 212 °F
ATI Allegheny Ludlum 440A Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
Thermal Conductivity 24.2 W/m-K
168 BTU-in/hr-ft²-°F
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..
Thermal Conductivity 24.2 W/m-K

@Temperature 20.0 - 100 °C
168 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..
Thermal Conductivity 24.2 W/m-K
168 BTU-in/hr-ft²-°F
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 10% cold work (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..
Thermal Conductivity 24.2 W/m-K

@Temperature 20.0 - 100 °C
168 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 10% cold work (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..
Thermal Conductivity 24.2 W/m-K
168 BTU-in/hr-ft²-°F
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 30% cold work (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..
Thermal Conductivity 24.2 W/m-K

@Temperature 20.0 - 100 °C
168 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 30% cold work (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..
Thermal Conductivity 24.2 W/m-K
168 BTU-in/hr-ft²-°F
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 70% cold work (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..
Thermal Conductivity 24.2 W/m-K

@Temperature 20.0 - 100 °C
168 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 70% cold work (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..
Thermal Conductivity 24.2 W/m-K

@Temperature 100 °C
168 BTU-in/hr-ft²-°F

@Temperature 212 °F
Latrobe LSS™ 440C Stainless Steel Knife (ASTM A276)
TLS 440C Stainless Knife Steel is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 60 HRC. The high carbon content results in a hard matrix and numero..
Thermal Conductivity 24.2 W/m-K
168 BTU-in/hr-ft²-°F
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 50% cold work (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..
Thermal Conductivity 24.2 W/m-K

@Temperature 20.0 - 100 °C
168 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 50% cold work (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..