Polymer Property : Thermal Conductivity = 24.2 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 3.48 W/m-K
24.2 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® H31D Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H31D is a single component, electrically conductive silver epoxy designed for die-bonding of semiconductors, including IC’s, resistors, capacitors, transistors, and d..