Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 25.9 W/m-K @Temperature 900 °C |
180 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes Hastelloy® C-2000® alloy, flat products Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 25.9 W/m-K | 180 BTU-in/hr-ft²-°F | |
SGL Carbon Group EK 200 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Thermal Conductivity | 25.9 W/m-K | 180 BTU-in/hr-ft²-°F | |
SGL Carbon Group EK 201 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Thermal Conductivity | 25.9 W/m-K | 180 BTU-in/hr-ft²-°F | |
SGL Carbon Group EK 203 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |