Polymer Property : Thermal Conductivity = 257.7 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 257.7 W/m-K
1788 BTU-in/hr-ft²-°F
Eagle Brass 19010 XP-150 Copper Nickel Silicon, 3/4 Hard
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
Thermal Conductivity 257.7 W/m-K
1788 BTU-in/hr-ft²-°F
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Extra Hard
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
Thermal Conductivity 257.7 W/m-K
1788 BTU-in/hr-ft²-°F
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Hard
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
Thermal Conductivity 257.7 W/m-K
1788 BTU-in/hr-ft²-°F
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Spring
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..