Polymer Property : Thermal Conductivity = 258 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 37.2 W/m-K
258 BTU-in/hr-ft²-°F
Eagle Brass 735 Nickel Silver 18%, 1/2 Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Thermal Conductivity 37.2 W/m-K
258 BTU-in/hr-ft²-°F
Eagle Brass 735 Nickel Silver 18%, 1/4 Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Thermal Conductivity 37.2 W/m-K
258 BTU-in/hr-ft²-°F
Eagle Brass 735 Nickel Silver 18%, 3/4 Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Thermal Conductivity 37.2 W/m-K
258 BTU-in/hr-ft²-°F
Eagle Brass 735 Nickel Silver 18%, Annealed
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Thermal Conductivity 37.2 W/m-K
258 BTU-in/hr-ft²-°F
Eagle Brass 735 Nickel Silver 18%, Extra Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Thermal Conductivity 37.2 W/m-K
258 BTU-in/hr-ft²-°F
Eagle Brass 735 Nickel Silver 18%, Extra Spring
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Thermal Conductivity 37.2 W/m-K
258 BTU-in/hr-ft²-°F
Eagle Brass 735 Nickel Silver 18%, Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Thermal Conductivity 37.2 W/m-K
258 BTU-in/hr-ft²-°F
Eagle Brass 735 Nickel Silver 18%, Spring
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company