Material Notes:
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.83 g/cc
0.319 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 60 - 70
60 - 70
Thickness > 0.020 Inch
Tensile Strength, Ultimate 386 - 476 MPa
56000 - 69000 psi
Tensile Strength, Yield 193 - 400 MPa
28000 - 58000 psi
0.2% offset
Elongation at Break 10 - 25 %
10 - 25 %
in 2 in.
Tensile Modulus 124 GPa
18000 ksi
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 37.2 W/m-K
258 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 72 %
72 %
Nickel, Ni 18 %
18 %
Zinc, Zn 10 %
10 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000223 ohm-cm
0.0000223 ohm-cm
Annealed