Thermal Properties Metric English Comments
Thermal Conductivity 0.259 - 0.540 W/m-K
1.80 - 3.75 BTU-in/hr-ft²-°F
Average value: 0.392 W/m-K Grade Count:6
Overview of materials for Polyamide-Imide, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp..
Thermal Conductivity 0.540 - 0.540 W/m-K

@Temperature 100 - 100 °C
3.75 - 3.75 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.540 W/m-K Grade Count:2
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi..