Thermal Properties Metric English Comments
Thermal Conductivity 0.692 W/m-K
4.80 BTU-in/hr-ft²-°F
Saint-Gobain Rulon® 945 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Thermal Conductivity 0.692 W/m-K
4.80 BTU-in/hr-ft²-°F
Saint-Gobain Rulon® 142 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Thermal Conductivity 0.691 W/m-K
4.80 BTU-in/hr-ft²-°F
ASTM F433
Sumitomo Bakelite North America 2008A Glass Reinforced Hardware Grade Epoxy
Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc.
Thermal Conductivity 0.692 W/m-K
4.80 BTU-in/hr-ft²-°F
CoorsTek PolyGlyde™ 3000 Self-Lubricating Seal
PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni..