Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 60.5 - 69.2 W/m-K | 420 - 480 BTU-in/hr-ft²-°F | |
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12†and in rounds up t.. |
|||
Thermal Conductivity | 60.5 W/m-K | 420 BTU-in/hr-ft²-°F | |
Eagle Brass 519 Phosphor Bronzes 6%, 1/2 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Thermal Conductivity | 60.5 W/m-K | 420 BTU-in/hr-ft²-°F | |
Eagle Brass 519 Phosphor Bronzes 6%, 1/4 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Thermal Conductivity | 60.5 W/m-K | 420 BTU-in/hr-ft²-°F | |
Eagle Brass 519 Phosphor Bronzes 6%, 3/4 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Thermal Conductivity | 60.5 W/m-K | 420 BTU-in/hr-ft²-°F | |
Eagle Brass 519 Phosphor Bronzes 6%, Annealed Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Thermal Conductivity | 60.5 W/m-K | 420 BTU-in/hr-ft²-°F | |
Eagle Brass 519 Phosphor Bronzes 6%, Extra Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Thermal Conductivity | 60.5 W/m-K | 420 BTU-in/hr-ft²-°F | |
Eagle Brass 519 Phosphor Bronzes 6%, Extra Spring Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Thermal Conductivity | 60.5 W/m-K | 420 BTU-in/hr-ft²-°F | |
Eagle Brass 519 Phosphor Bronzes 6%, Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Thermal Conductivity | 60.5 W/m-K | 420 BTU-in/hr-ft²-°F | |
Eagle Brass 519 Phosphor Bronzes 6%, Spring Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Thermal Conductivity | 60.7 W/m-K @Temperature 27.0 - 100 °C |
420 BTU-in/hr-ft²-°F @Temperature 80.6 - 212 °F |
|
Carlson C 200 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |
|||
Thermal Conductivity | 60.7 W/m-K @Temperature 27.0 - 100 °C |
420 BTU-in/hr-ft²-°F @Temperature 80.6 - 212 °F |
|
Carlson C 201 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |