Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 5.76 - 6.48 W/m-K | 40.0 - 45.0 BTU-in/hr-ft²-°F | |
Master Bond EP41S Fast Curing Epoxy Features Chemical Resistance Description: Master Bond EP41S is a two component epoxy resin compound for durable, high performance, tough, high strength coatings, liners and sealants with outstanding resistance to organic solven.. |