Polymer Property : Thermal Conductivity = 6.48 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 5.76 - 6.48 W/m-K
40.0 - 45.0 BTU-in/hr-ft²-°F
Master Bond EP41S Fast Curing Epoxy Features Chemical Resistance
Description: Master Bond EP41S is a two component epoxy resin compound for durable, high performance, tough, high strength coatings, liners and sealants with outstanding resistance to organic solven..