Thermal Properties Metric English Comments
Thermal Conductivity 8.10 W/m-K
56.2 BTU-in/hr-ft²-°F
in-plane, ø25*0.4mm disc; ASTM E 1461-07
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6
LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant
Thermal Conductivity 8.10 W/m-K
56.2 BTU-in/hr-ft²-°F
in-plane, ø25*0.4mm disc; ASTM E 1461-07
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound
Thermal Conductivity 8.10 W/m-K
56.2 BTU-in/hr-ft²-°F
in-plane, ø25*0.4mm disc; ASTM E 1461-07
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral filled PA6 non-halogen FR compound