Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 8.10 W/m-K | 56.2 BTU-in/hr-ft²-°F | in-plane, ø25*0.4mm disc; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant |
|||
Thermal Conductivity | 8.10 W/m-K | 56.2 BTU-in/hr-ft²-°F | in-plane, ø25*0.4mm disc; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Thermal Conductivity | 8.10 W/m-K | 56.2 BTU-in/hr-ft²-°F | in-plane, ø25*0.4mm disc; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 non-halogen FR compound |