Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.918 W/m-K | 6.37 BTU-in/hr-ft²-°F | ASTM C177 |
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK) Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent .. |
|||
Thermal Conductivity | 0.918 W/m-K | 6.37 BTU-in/hr-ft²-°F | ASTM C177 |
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Thermal Conductivity | 0.918 W/m-K | 6.37 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho.. |