Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Ensinger
Trade Name Tecapeek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent flexural, impact, and tensile characteristics Very high continuous working temp Very high heat distortion temp Exceptional chemical resistance Superior dielectric at high temperatures and frequencies Good radiation resistance Outstanding wear and abrasion resistance Low smoke and toxic gas emissions Excellent hydrolysis resistance Information provided by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
at 24 hours; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 107
107
ASTM D785
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
ASTM D638
Tensile Modulus 12.999 GPa
1885.4 ksi
1 % Sec; ASTM D638
Flexural Strength 318 MPa
46100 psi
ASTM D790
Flexural Modulus 12.755 GPa
1850.0 ksi
Tangent; ASTM D790
Compressive Strength 240 MPa
34800 psi
ASTM D695
Shear Strength 97.2 MPa
14100 psi
Ultimate; ASTM D3846
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.22
0.22
1200 in/min, 155 lbs Load; ASTM D1894-95
Limiting Pressure Velocity 13.5 MPa-m/sec
385000 psi-ft/min
1200 in/min
Thermal Properties Metric English Comments
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 °C
8.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.918 W/m-K
6.37 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 334 °C
633 °F
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 316 °C
600 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 140000 ohm-cm
140000 ohm-cm
ASTM D257
Users viewing this material also viewed the following: