Thermal Properties Metric English Comments
Thermal Conductivity 0.940 - 0.940 W/m-K

@Temperature 100 - 100 °C
6.52 - 6.52 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.940 W/m-K Grade Count:1
Overview of materials for Phenolic; Unreinforced; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of..