Polymer Property : Thermal Conductivity = 6.59 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.950 W/m-K

@Temperature 80.0 °C
6.59 BTU-in/hr-ft²-°F

@Temperature 176 °F
Z Direction; ASTM C518
Rogers Corporation RO3010 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Features and Benefits:
Thermal Conductivity 0.950 W/m-K
6.59 BTU-in/hr-ft²-°F
ASTM D5470
Parker Chomerics THERM-A-FORM 1642 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Thermal Conductivity 0.950 W/m-K
6.59 BTU-in/hr-ft²-°F
Average; ISO 22007-4
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c..
Thermal Conductivity 0.950 W/m-K
6.59 BTU-in/hr-ft²-°F
Average; ISO 22007-4
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
Thermal Conductivity 0.950 W/m-K
6.59 BTU-in/hr-ft²-°F
Average; ISO 22007-4
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant..
Thermal Conductivity 0.950 W/m-K

@Temperature 23.0 °C
6.59 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
Average; ISO/CD 22007-4
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont..
Thermal Conductivity 0.950 W/m-K

@Temperature 23.0 °C
6.59 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
Average; ISO/CD 22007-4
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
Thermal Conductivity 0.950 W/m-K
6.59 BTU-in/hr-ft²-°F
Schott N-K5 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.950 W/m-K
6.59 BTU-in/hr-ft²-°F
Schott N-SF11 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.950 W/m-K
6.59 BTU-in/hr-ft²-°F
Schott N-SF4 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.950 W/m-K
6.59 BTU-in/hr-ft²-°F
Dow Corning SE 4430 KIT
Two-part, thermally conductive elastomer, soft, good thermal conducitvity, UL 94 V-0 rating, low viscosity.Information provided by Dow Corning
Thermal Conductivity 0.950 W/m-K
6.59 BTU-in/hr-ft²-°F
Schott N-KZFS5 Glass
Information Provided by SCHOTT North America, Inc.