Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 93.0 W/m-K | 645 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 245C Castings (UNS C82600) Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula.. |
|||
Thermal Conductivity | 93.0 W/m-K | 645 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 245CT Castings (UNS C82600) Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula.. |
|||
Thermal Conductivity | 93.0 W/m-K @Temperature 20.0 °C |
645 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Not listed in the ASTM.Information provided by AK Steel |
|||
Thermal Conductivity | 93.0 W/m-K | 645 BTU-in/hr-ft²-°F | |
AK Steel ASTM A 424 Type III, I-F Enamel Enameling Carbon Steel I-F Enameling Steel is a vacuum degassed, titanium stabilized steel. I-F Enameling Steel can be used for ground coat and two coat-one fire porcelain enameling systems. It is not recommended for us.. |
|||
Thermal Conductivity | 93.0 W/m-K | 645 BTU-in/hr-ft²-°F | |
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Interstitial Free (I-F) steels are made by adding titanium and/or niobium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Thermal Conductivity | 93.0 W/m-K | 645 BTU-in/hr-ft²-°F | |
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F) steels are made by adding titanium and/or niobium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Thermal Conductivity | 93.0 W/m-K | 645 BTU-in/hr-ft²-°F | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Interstitial Free (I-F) steels are made by adding titanium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel |
|||
Thermal Conductivity | 93.0 W/m-K | 645 BTU-in/hr-ft²-°F | |
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Extra Deep Drawing Steel (EDDS), Standard Grade Interstitial Free (I-F) steels are made by adding titanium and/or columbium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel |
|||
Thermal Conductivity | 93.0 W/m-K | 645 BTU-in/hr-ft²-°F | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Interstitial Free (I-F®) steels are made by adding titanium and/or columbium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Thermal Conductivity | 93.0 W/m-K | 645 BTU-in/hr-ft²-°F | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F®) steels are made by adding titanium and/or columbium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Thermal Conductivity | 93.0 W/m-K @Temperature 20.0 °C |
645 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 50F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Information provided by AK Steel |
|||
Thermal Conductivity | 93.0 W/m-K @Temperature 20.0 °C |
645 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Information provided by AK Steel |
|||
Thermal Conductivity | 93.0 W/m-K | 645 BTU-in/hr-ft²-°F | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F) steels are made by adding titanium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel |
|||
Thermal Conductivity | 93.0 W/m-K | 645 BTU-in/hr-ft²-°F | |
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F) steels are made by adding titanium and/or columbium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel |