Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AK Steel ASTM A 1011, Class 2 Formable, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F)

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer AK Steel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel ASTM A 1011, Class 2 Formable, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Not listed in the ASTM.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.87 g/cc

@Temperature 20.0 °C
0.284 lb/in³

@Temperature 68.0 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
Tensile Strength, Yield >= 380 MPa
>= 55100 psi
Elongation at Break >= 20 %
>= 20 %
Modulus of Elasticity 200 GPa

@Temperature 20.0 °C
29000 ksi

@Temperature 68.0 °F
Thermal Properties Metric English Comments
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.481 J/g-°C

@Temperature 50.0 - 100 °C
0.115 BTU/lb-°F

@Temperature 122 - 212 °F
Thermal Conductivity 93.0 W/m-K

@Temperature 20.0 °C
645 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
Users viewing this material also viewed the following: