Thermal Properties Metric English Comments
Thermal Conductivity 135 - 210 W/m-K
937 - 1460 BTU-in/hr-ft²-°F
H.C. Starck WCu 85/15 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
Thermal Conductivity 135 - 150 W/m-K
937 - 1040 BTU-in/hr-ft²-°F
temper T651
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing ..
Thermal Conductivity 135 W/m-K
937 BTU-in/hr-ft²-°F
CMW® ELKONITE® 40W3 Infiltrated Tungsten Copper material ASTM B702
For vacuum switch contacts, low expansion structural members.Information provided by CMW Inc.