Thermal Properties Metric English Comments
Thermal Conductivity 200 - 210 W/m-K
1390 - 1460 BTU-in/hr-ft²-°F
z direction
MarkeTech Cu/Mo/Cu 1:2:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
Thermal Conductivity 135 - 210 W/m-K
937 - 1460 BTU-in/hr-ft²-°F
H.C. Starck WCu 85/15 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..