Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 1200 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 142 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 200 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 75 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 1000 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 1200 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 1400 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 75 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 750 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 300 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 750 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 142 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 300 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 400 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 48 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 500 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 900 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 92 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MLB Polyester Film, 48 Gauge Product Description: Mylar® MLB is an uncoated, transparent, polyester film designed for use as a component of a lamination structure and may be suitable for use in medical applications. Mylar® ML.. |
|||
Maximum Service Temperature, Inert | -73.3 °C | -100 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 200 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |