Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 130 °C
266 °F
Haysite H722 Polyester, Glass Reinforced
H722 is an all-purpose GPO-1 fiberglass mat reinforced thermoset polyester molded sheet. Available in thicknesses ranging from .031" - 2.00". Standard color - Natural. Meets Gov't Specs - LP-509, ..
Maximum Service Temperature, Inert 130 °C
266 °F
ASTM D794
Techmer ES Plastiblend® TPX-HTN-000AA
Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc.
Maximum Service Temperature, Inert 130 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
266 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Elektro-Isola Etronax DN Phenolic, Cotton Fabric Reinforcement, Brown, Tubes
Description: A strong and tough material. Very low water absorption and the lowest swelling in water. Very good low-friction material. High wear resistance in aggressive and dust-filled environments..
Maximum Service Temperature, Inert 130 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
266 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets
Description: This material is exceptionally strong and tough. Very low water absorption and the lowest swelling in water. High resistance to chemicals, including SF6 gas. Applications: Can be used i..
Maximum Service Temperature, Inert 130 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
266 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Sheets
Description: Melamine-based composite material reinforced with glass fabric. High arc resistance and tracking resistance. Flame-resistant. Self-extinguishing.Information provided by Elektro-Isola
Maximum Service Temperature, Inert 130 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
266 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Tubes
Description: Mechanical and electrical applications. Arc-resistant and tracking-resistant material. Good flame resistance. Self-extinguishing. Halogen-free. Lower high-voltage values and insulation ..