Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 149 - 232 °C
300 - 450 °F
Average value: 226 °C Grade Count:92
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Maximum Service Temperature, Inert 149 °C
300 °F
Arlon 47568R055E 0.0075" Cured Silicone Rubber/Fiberglass/Acrylic PSA Laminate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassSide 2: Acrylic PSAInterleave: PolypropyleneThis data represents typical values for the production material and sho..
Maximum Service Temperature, Inert 149 °C
300 °F
Arlon R32458R0055E 0.0075" Cured Silicone Rubber with Fiberglass Substrate and Acrylic PSA
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassSide 2: Acrylic PSAInterleave: PolypropyleneThis data represents typical values for the production material and sh..