Arlon R32458R0055E 0.0075" Cured Silicone Rubber with Fiberglass Substrate and Acrylic PSA

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R32458R0055E 0.0075" Cured Silicone Rubber with Fiberglass Substrate and Acrylic PSA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassSide 2: Acrylic PSAInterleave: PolypropyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 50.8 microns
2.00 mil
Side 1; Arlon SQA-TMS-003
50.8 microns
2.00 mil
Side 2; Arlon SQA-TMS-003
88.9 microns
3.50 mil
Substrate; Arlon SQA-TMS-003
191 microns
7.50 mil
Overall thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Silicone Property; ASTM D2240
Tensile Strength 6.21 MPa
900 psi
Silicone Property; ASTM D412
Elongation at Break 600 %
600 %
Silicone Property; ASTM D412
Peel Strength 0.0877 kN/m
0.500 pli
Bond Strength; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 149 °C
300 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 23.9 °C
12.0 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 6.5
Arlon SQA-TMS-025