Polymer Property : Maximum Service Temperature, Inert = 2100 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 1150 - 1600 °C
2100 - 2910 °F
Inert/Vacuum
Momentive Performance Materials HBR Hot-Pressed Boron Nitride
Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom..
Maximum Service Temperature, Inert 1150 °C
2100 °F
Aremco AREMCOLOX™ 502-1600 (94%) Machinable Boron Nitride 94%
Hot-pressed 94% boron nitride. High thermal conductivity. Easily machined. Non-reactive in molten salts, aluminum and other metals. Plates from 1/4" to 1" thick; rods from 1/4" to 3" diameter; b..