Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 550 - 1600 °C | 1020 - 2910 °F | Inert/Vacuum |
Momentive Performance Materials HBN Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Maximum Service Temperature, Inert | 1150 - 1600 °C | 2100 - 2910 °F | Inert/Vacuum |
Momentive Performance Materials HBR Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |