Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 160 °C | 320 °F | |
Haysite H900 Polyester, Glass Reinforced H900 is recognized throughout the world as a reliable, consistent GPO-3 material. Standard size sheets are available in thicknesses ranging from .094" to 2.00". H900 also exhibits excellent smoke,.. |
|||
Maximum Service Temperature, Inert | 160 °C | 320 °F | ASTM D794 |
Techmer ES Plastiblend® TPX-HTN-000AB 15% Glass Filled Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Maximum Service Temperature, Inert | 160 °C | 320 °F | ASTM D794 |
Techmer ES Plastiblend® TPX-HTN-000CA Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Maximum Service Temperature, Inert | 160 °C | 320 °F | ASTM D794 |
Techmer ES Plastiblend® TPX-HTN-000CB 15% Glass Filled Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Maximum Service Temperature, Inert | 160 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
320 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola G-Etronax EP 22 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc.. |
|||
Maximum Service Temperature, Inert | 160 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
320 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c.. |