Polymer Property : Maximum Service Temperature, Air = 108 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 108 °C
226 °F
Continuous Use
Polyram PlusTek PB507 Nylon 6, Flame Retardant
Flame retardant halogen free polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Maximum Service Temperature, Air 108 °C
226 °F
Martens Dimensional Stability
CMT Materials METAPOR® HD 100 AL Air Permeable Material
METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi..
Maximum Service Temperature, Air 108 °C
226 °F
Martens Dimensional Stability
CMT Materials METAPOR® BF 100 AL Air Permeable Material
METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi..
Maximum Service Temperature, Air 108 °C
226 °F
Deflection Temp at unknown load
Abatron AboCast 8103-22 High-Performance Dielectric Epoxy
AboCast 8103-22 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system is used in..
Maximum Service Temperature, Air 108 - 210 °C
226 - 410 °F
Average value: 145 °C Grade Count:10
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..