Polymer Property : Maximum Service Temperature, Air = 152 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 152 °C
306 °F
Heat Resistance per Montell
LyondellBasell Adflexâ„¢ Q 401 F TPO Resin
Thermoplastic olefin resin wit slip and antiblock for air quenched blown film, excellent heat resistance, excellent puncture resistance, great tear resistance, FDA acceptableApplications: films requ..
Maximum Service Temperature, Air 152 °C
306 °F
Heat Resistance; ASTM D570D
Plenco 00755 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755..
Maximum Service Temperature, Air 152 °C
306 °F
5000 hours Thermal Index; IEC 60216/ISO 27-1/-2
DSM Stanyl® TW341-B PA46
Heat Stabilized, Lubricated
Maximum Service Temperature, Air 152 °C
306 °F
5000 hours Thermal Index; IEC 60216/ISO 527-1/-2
DSM Stanyl® TW341-N PA46
Heat Stabilized, Lubricated
Maximum Service Temperature, Air 152 °C
306 °F
Heat Resistance; ASTM D570D
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Maximum Service Temperature, Air 152 °C
306 °F
5000 hours Thermal Index; IEC 60216/ISO 527-1/-2
DSM Stanyl® TS200F6 PA46-GF30
30% Glass Reinforced