Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 850 °C | 1560 °F | Dry Air |
Outokumpu 4724 High Temperature Ferritic Stainless Steel Truly stainless high temperature grade with 13% chromium. Not critical in terms of embrittlement.Applications: Mostly used in high temperature applications with sulphurous atmospheres and/or low te.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | |
Pyrotek AF-8 Mineral Fiber Paper Pyrotek's AF-8 Mineral Fiber Paper is a low shot paper used in high temperature gasketing and as an insulating parting agent between refractory and metal work. It is a soft, flexible, clean pa.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | Continuous |
Pyrotek Pyrite N-14 Refractory Board Pyrotek N-14 is a fiberglass reinforced calcium silicate board specifically developed for the non-ferrous industry. The superior strength and unique formulation of Pyrotek N-14 makes it the preferr.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | Continuous |
Pyrotek Pyrite N-17 Refractory Board Pyrotek N-17 is a graphite fiber reinforced, high purity, calcium silicate board developed exclusively for the non-ferrous casting industry. The patented formulation of Pyrotek N-17 makes it good i.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | |
Pyrotek Pyrocast AR70 Low-Density Refractory Castable Pyrocast AR70 refractory castable is a high-strength, low-density refractory well suited for specific aluminum foundry applications.ApplicationsSprue Bushings for low pressure die casting Intermedia.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | |
Pyrotek Pyrocast HD Castable Refractory Pyrocast HD is an insulating castable which is particularly suitable in applications where a combination of low thermal conductivity and long service life is required.ApplicationsLaunder lining Hot-.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | Continuous |
Pyrotek Thermollite Insulating Refractory Shapes for Molten Aluminum Thermollite has been specifically developed for direct contact with molten aluminum and its various alloys. Thermollite provides the specific advantage of reducing heat loss in melt transfer applic.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | resists repeated cycles |
MarkeTech Cu/Mo/Cu 1:1:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | resists repeated cycles |
MarkeTech Cu/Mo/Cu 1:2:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | resists repeated cycles |
MarkeTech Cu/Mo/Cu 1:3:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | resists repeated cycles |
MarkeTech Cu/Mo/Cu 1:4:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | resists repeated cycles |
MarkeTech Cu/Mo/Cu 1:5:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | resists repeated cycles |
MarkeTech Cu/Mo/Cu 13:74:13 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | resists repeated cycles |
MarkeTech Cu/Mo70-Cu30/Cu 1:4:1 Laminated Sheet Cu/Mo/Cu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated he.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | Oxidizing Environments |
Momentive Performance Materials Boron Nitride (BN) Spray BN aerosol spray delivers high purity, extremely fine, BN crystals in a fast drying solvent-base carrier. It produces a smooth coating with even film build that is virtually binderless.Uses of GE A.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | Oxidizing Environments |
Momentive Performance Materials EPC Boron Nitride (BN) Water Based Coating Solids content > 9%. Can be applied by brush, roller, dipping, or spraying. Can be applied to either hot or cold services although use of water based coatings on surfaces greater than 100°C is .. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | Oxidizing Environments |
Momentive Performance Materials FPC APC Boron Nitride (BN)/Al2O3 Water Based Coating Solids content > 25%. Can be applied by brush, roller, dipping, or spraying. Can be applied to either hot or cold services although use of water based coatings on surfaces greater than 100°C is.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | oxidizing atmosphere |
Momentive Performance Materials HBC Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | oxidizing atmosphere |
Momentive Performance Materials HBR Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | oxidizing atmosphere |
Momentive Performance Materials HBT Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | Oxidizing Environments |
Momentive Performance Materials HPC Boron Nitride (BN)/TiO2 Water Based Coating Solids content > 25%. Can be applied by brush, roller, dipping, or spraying. Can be applied to either hot or cold services although use of water based coatings on surfaces greater than 100°C is.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | Oxidizing |
Momentive Performance Materials FPD Boron Nitride (BN) Coating Can be applied by brush, roller, dipping, or spraying. Can be applied to either hot or cold services although use of water based coatings on surfaces greater than 100°C is not recommended. Mult.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | |
Skamol Group SKAMOCAST 14-105 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | |
CeramTec ZN 40 Zirconia, ZrO2-MgO ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma.. |
|||
Maximum Service Temperature, Air | 849 °C | 1560 °F | |
Aremco Pyro-Paint™ 634-BN (SC) High Temperature Refractory Coating This highly-filled boron nitride solution is extremely lubricious and inert. It is non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN(SC) .. |
|||
Maximum Service Temperature, Air | 849 °C | 1560 °F | |
Aremco Pyro-Paint™ 634-BN High Temperature Refractory Coating This highly-filled boron nitrite solution is extremely lubricious and inert. They are non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN f.. |
|||
Maximum Service Temperature, Air | 850 °C | 1560 °F | Oxidizing Environments |
Momentive Performance Materials GPC Boron Nitride (BN) Water Based Coating Solids content > 25%. Can be applied by brush, roller, dipping, or spraying. Can be applied to either hot or cold services although use of water based coatings on surfaces greater than 100°C is n.. |