Aremco Pyro-Paint™ 634-BN (SC) High Temperature Refractory Coating

Category Ceramic , Nitride
Manufacturer Aremco
Trade Name Pyro-Paint™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Pyro-Paint™ 634-BN (SC) High Temperature Refractory Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This highly-filled boron nitride solution is extremely lubricious and inert. It is non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN(SC) for softer, lubricious coat.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Density 1.14 g/cc
0.0411 lb/in³
Solids Content 27.5 %
27.5 %
volume
28.5 %
28.5 %
weight
pH 4.0 - 5.0
4.0 - 5.0
Coating pH
Viscosity 10.0 - 100 cP
10.0 - 100 cP
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 849 °C
1560 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
>2 Hour Air Set Required Prior to Curing
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color White
Coverage ft2/gal 440
Theoretical Coverage at 1 mil dry film thickness
Thinner 634 BNSC-T
Weight/Gallon 9.5 lbs