Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 92.0 °C | 198 °F | Deflection Temperature with load unspecified; ASTM D648 |
Plaskolite PL-24 Acrylic Resin For injection molding. An unlubricated version of PL-25 extrusion grade pellets. Highest molecular weight, maximum heat resistance.Information supplied by the manufacturer. |
|||
Maximum Service Temperature, Air | 92.0 °C | 198 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. (dry sample) |
Omnia Plastica Akulon® PA 66.6 - Akulon GX - at 50% RH Copolymer of nylon with excellent mechanical features, it combines the good impact resistances of PA6 as well as the higher stiffness of PA66. For this reason it machines very well on automatic tool.. |
|||
Maximum Service Temperature, Air | 92.0 °C | 198 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. |
Omnia Plastica Akulon® PA 66.6 Akulon GX - Dry Copolymer of nylon with excellent mechanical features, it combines the good impact resistances of PA6 as well as the higher stiffness of PA66. For this reason it machines very well on automatic tool.. |
|||
Maximum Service Temperature, Air | 92.0 - 244 °C | 198 - 471 °F | Average value: 148 °C Grade Count:8 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Maximum Service Temperature, Air | 92.0 °C | 198 °F | Heat Distortion Temp |
Lucky EF-940 Acrylic, Injection/Extrusion Grade Extrusion and injection grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capa.. |
|||
Maximum Service Temperature, Air | 92.0 °C | 198 °F | Deflection Temp; Load not reported; ASTM D648 |
Lucky EF-940 Acrylic, Injection/Extrusion Grade Extrusion and injection grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capa.. |
|||
Maximum Service Temperature, Air | 92.2 °C | 198 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSI 935E Polystyrene Polystyrene 935E is a high impact polystyrene exhibiting exceptional toughness for sheet and thermoforming applications.This polymer is an excellent choice for cups, food packaging, custom sheet and.. |
|||
Maximum Service Temperature, Air | 92.2 °C | 198 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSI 975E Polystyrene Polystyrene 975E is a high impact polystyrene designed for extrusion/thermoforming applications. The food ESCR properties of 975E dictate its use for dairy applications that are subjected to high bu.. |
|||
Maximum Service Temperature, Air | 92.0 °C | 198 °F | Deflection temperature; load unknown. |
Abatron AboCast 50-6/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months. |
|||
Maximum Service Temperature, Air | 92.0 - 102 °C | 198 - 216 °F | Softening point |
Mitsui MILEX™ RN-2410MB Acrylic Rubber Modified Phenolic Resin
(discontinued **) The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic .. |
|||
Maximum Service Temperature, Air | 92.0 - 102 °C | 198 - 216 °F | Softening point |
Mitsui MILEX™ RX-2325C Low Silicone Rubber Modified Phenolic Resin
(discontinued **) The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic .. |