Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 95.0 - 102 °C | 203 - 216 °F | Softening point |
Mitsui MILEXâ„¢ RS-2210MB Silicone Rubber Modified Phenolic Resin The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad.. |
|||
Maximum Service Temperature, Air | 92.0 - 102 °C | 198 - 216 °F | Softening point |
Mitsui MILEX™ RN-2410MB Acrylic Rubber Modified Phenolic Resin
(discontinued **) The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic .. |
|||
Maximum Service Temperature, Air | 92.0 - 102 °C | 198 - 216 °F | Softening point |
Mitsui MILEX™ RX-2325C Low Silicone Rubber Modified Phenolic Resin
(discontinued **) The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic .. |