Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 104 °C | 219 °F | Modified ISO 2796-1980; Typical maximum temperature to which parts can be exposed short term (1 hour) without significant deformation (<1%). |
NOVA Chemicals Dytherm® 140R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Modified ISO 2796-1980; Typical maximum temperature to which parts can be exposed short term (1 hour) without significant deformation (<1%). |
NOVA Chemicals Dytherm® 150F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Modified ISO 2796-1980; Typical maximum temperature to which parts can be exposed short term (1 hour) without significant deformation (<1%). |
NOVA Chemicals Dytherm® 150R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Modified ISO 2796-1980; Typical maximum temperature to which parts can be exposed short term (1 hour) without significant deformation (<1%). |
NOVA Chemicals Dytherm® 170F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Modified ISO 2796-1980; Typical maximum temperature to which parts can be exposed short term (1 hour) without significant deformation (<1%). |
NOVA Chemicals Dytherm® 170R Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Service |
3M FP010602 Matte White Polypropylene Label Product 3M™ Matte White Polypropylene Label Products FP010602, FP010609 and FP017802 are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Service |
3M FP017802 Matte White Polypropylene Label Product 3M™ Matte White Polypropylene Label Products FP010602, FP010609 and FP017802 are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Deflection Temp at unknown load |
Abatron AboCast 8103-13 One-Component Epoxy AboCast 8103-13 is the low-viscosity one-component clear epoxy system with deep impregnation that offers high performance at relatively high temperatures. It is best for thin-wall casting. Suggested.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4004 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4008 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4016 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4026 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4032 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4052 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4056 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4085 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Service |
3M FP010609 Matte White Polypropylene Label Product 3M™ Matte White Polypropylene Label Products FP010602, FP010609 and FP017802 are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3.. |