Material Notes:
AboCast 8103-13 is the low-viscosity one-component clear epoxy system with deep impregnation that offers high performance at relatively high temperatures. It is best for thin-wall casting. Suggested Uses: Casting; Potting; Encapsulating; Embedding applications where 2-component systems can not be used; Electronic and structural components, patterns, and medical equipment; Coating; Impregnation; Resurfacing; Insulation; Bonding metal, ceramics, glass, and most rigid materials; Assembly; Patching; and Filling.
Physical Properties Metric English Comments
Viscosity 600 cP
600 cP
Mechanical Properties Metric English Comments
Hardness, Rockwell M 98
98
Tensile Strength at Break 44.1 MPa
6400 psi
Elongation at Break 3.3 %
3.3 %
Flexural Strength 92.4 MPa
13400 psi
Flexural Modulus 2.69 GPa
390 ksi
Compressive Strength 90.3 MPa
13100 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 104 °C
219 °F
Deflection Temp at unknown load
Electrical Properties Metric English Comments
Volume Resistivity 3.62e+12 ohm-cm
3.62e+12 ohm-cm
C 96/23/96
2.58e+15 ohm-cm
2.58e+15 ohm-cm
"A"
Surface Resistance 7.38e+11 ohm
7.38e+11 ohm
C 96/23/96
2.36e+15 ohm
2.36e+15 ohm
Cond. A
Dielectric Constant 3.1

@Frequency 1.00e+6 Hz
3.1

@Frequency 1.00e+6 Hz
A
3.27

@Frequency 60.0 Hz
3.27

@Frequency 60.0 Hz
A
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 150 - 160 °C
1.00 - 2.00 hour

@Temperature 302 - 320 °F
60.0 - 240 min

@Temperature 160 - 180 °C
1.00 - 4.00 hour

@Temperature 320 - 356 °F
optional
Pot Life 180 min

@Temperature 100 °C
180 min

@Temperature 212 °F
Shelf Life 5.00 - 8.00 Month