Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 244 °C | 471 °F | Heat Resistance; ASTM D570D |
Plenco 6582 Phenolic, Briquette, Injection Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |