Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 - 250 °C
302 - 482 °F
Average value: 211 °C Grade Count:12
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
Maximum Service Temperature, Air 90.0 - 250 °C
194 - 482 °F
Average value: 133 °C Grade Count:15
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Maximum Service Temperature, Air 90.0 - 250 °C
194 - 482 °F
Average value: 164 °C Grade Count:24
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Maximum Service Temperature, Air 90.0 - 250 °C
194 - 482 °F
Average value: 164 °C Grade Count:23
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Maximum Service Temperature, Air 135 - 250 °C
275 - 482 °F
Average value: 186 °C Grade Count:6
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..
Maximum Service Temperature, Air 110 - 250 °C
230 - 482 °F
Average value: 160 °C Grade Count:3
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Maximum Service Temperature, Air 80.0 - 250 °C
176 - 482 °F
Average value: 140 °C Grade Count:6
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Maximum Service Temperature, Air 230 - 250 °C
446 - 482 °F
Softening Range
Huntsman DT 3355 Matting Agent
Color: Off-whiteComments/Applications: Reactive matting agent for low gloss epoxy and epoxy/polyester hybrid powder formulations.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals ha..
Maximum Service Temperature, Air 150 - 250 °C
302 - 482 °F
Average value: 184 °C Grade Count:5
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Maximum Service Temperature, Air 130 - 250 °C
266 - 482 °F
Average value: 163 °C Grade Count:8
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..
Maximum Service Temperature, Air 93.0 - 250 °C
199 - 482 °F
Average value: 178 °C Grade Count:6
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..