Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 40% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.39 - 1.62 g/cc
0.0502 - 0.0585 lb/in³
Average value: 1.51 g/cc Grade Count:45
Filler Content 40.0 - 50.0 %
40.0 - 50.0 %
Average value: 44.3 % Grade Count:6
Water Absorption 0.00700 - 6.00 %
0.00700 - 6.00 %
Average value: 4.17 % Grade Count:26
Moisture Absorption at Equilibrium 0.850 - 2.00 %
0.850 - 2.00 %
Average value: 1.61 % Grade Count:23
Water Absorption at Saturation 2.75 - 5.00 %
2.75 - 5.00 %
Average value: 3.92 % Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.0180 cm/cm
0.00100 - 0.0180 in/in
Average value: 0.00226 cm/cm Grade Count:36
Linear Mold Shrinkage, Transverse 0.00300 - 0.0120 cm/cm
0.00300 - 0.0120 in/in
Average value: 0.00596 cm/cm Grade Count:27
Mechanical Properties Metric English Comments
Ball Indentation Hardness 100 - 325 MPa
14500 - 47100 psi
Average value: 223 MPa Grade Count:21
Tensile Strength, Ultimate 50.0 - 265 MPa
7250 - 38400 psi
Average value: 187 MPa Grade Count:44
140 - 150 MPa

@Temperature 80.0 - 80.0 °C
20300 - 21800 psi

@Temperature 176 - 176 °F
Average value: 128 MPa Grade Count:4
110 - 110 MPa

@Temperature >=130 °C
16000 - 16000 psi

@Temperature >=266 °F
Average value: 128 MPa Grade Count:1
110 - 110 MPa

@Time 1.80e+7 - 7.20e+7 sec
16000 - 16000 psi

@Time 5000 - 20000 hour
Average value: 128 MPa Grade Count:1
Elongation at Break 1.50 - 16.0 %
1.50 - 16.0 %
Average value: 3.45 % Grade Count:43
2.40 - 2.80 %

@Temperature 80.0 - 80.0 °C
2.40 - 2.80 %

@Temperature 176 - 176 °F
Average value: 2.70 % Grade Count:4
Elongation at Yield 3.00 - 6.00 %
3.00 - 6.00 %
Average value: 4.60 % Grade Count:3
Modulus of Elasticity 3.00 - 17.8 GPa
435 - 2580 ksi
Average value: 12.3 GPa Grade Count:38
8.05 - 10.0 GPa

@Temperature 80.0 - 80.0 °C
1170 - 1450 ksi

@Temperature 176 - 176 °F
Average value: 8.63 GPa Grade Count:4
Flexural Yield Strength 45.0 - 380 MPa
6530 - 55100 psi
Average value: 285 MPa Grade Count:18
240 - 260 MPa

@Temperature 80.0 - 80.0 °C
34800 - 37700 psi

@Temperature 176 - 176 °F
Average value: 253 MPa Grade Count:4
Flexural Modulus 8.62 - 16.2 GPa
1250 - 2350 ksi
Average value: 12.5 GPa Grade Count:17
8.30 - 9.50 GPa

@Temperature 80.0 - 80.0 °C
1200 - 1380 ksi

@Temperature 176 - 176 °F
Average value: 9.10 GPa Grade Count:3
Izod Impact, Notched 0.801 - 1.80 J/cm
1.50 - 3.37 ft-lb/in
Average value: 1.45 J/cm Grade Count:3
Izod Impact, Notched (ISO) 8.50 - 57.0 kJ/m²
4.04 - 27.1 ft-lb/in²
Average value: 18.0 kJ/m² Grade Count:10
11.0 - 48.0 kJ/m²

@Temperature -40.0 - -20.0 °C
5.23 - 22.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 20.5 kJ/m² Grade Count:2
Izod Impact, Unnotched (ISO) 50.0 - 82.0 kJ/m²
23.8 - 39.0 ft-lb/in²
Average value: 62.7 kJ/m² Grade Count:7
45.0 - 74.0 kJ/m²

@Temperature -30.0 - -30.0 °C
21.4 - 35.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 61.3 kJ/m² Grade Count:3
Charpy Impact Unnotched 4.00 J/cm² - NB
19.0 ft-lb/in² - NB
Average value: 8.17 J/cm² Grade Count:34
3.00 J/cm² - NB

@Temperature -40.0 - 30.0 °C
14.3 ft-lb/in² - NB

@Temperature -40.0 - 86.0 °F
Average value: 6.90 J/cm² Grade Count:26
Charpy Impact, Notched 0.400 - 4.50 J/cm²
1.90 - 21.4 ft-lb/in²
Average value: 2.03 J/cm² Grade Count:34
0.300 - 4.50 J/cm²

@Temperature -30.0 - 30.0 °C
1.43 - 21.4 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.92 J/cm² Grade Count:25
Thermal Properties Metric English Comments
CTE, linear 10.0 - 30.0 µm/m-°C
5.56 - 16.7 µin/in-°F
Average value: 19.6 µm/m-°C Grade Count:26
CTE, linear, Transverse to Flow 50.0 - 136 µm/m-°C
27.8 - 75.6 µin/in-°F
Average value: 78.2 µm/m-°C Grade Count:22
Melting Point 235 - 310 °C
455 - 590 °F
Average value: 258 °C Grade Count:38
Maximum Service Temperature, Air 90.0 - 250 °C
194 - 482 °F
Average value: 164 °C Grade Count:23
Hot Ball Pressure Test 123 - 220 °C
253 - 428 °F
Average value: 185 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 220 - 261 °C
428 - 502 °F
Average value: 243 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 145 - 280 °C
293 - 536 °F
Average value: 233 °C Grade Count:40
Deflection Temperature at 8.0 MPa 60.0 - 235 °C
140 - 455 °F
Average value: 194 °C Grade Count:27
Flammability, UL94 HB - 5VB
HB - 5VB
Grade Count:27
Glow Wire Test 650 - 960 °C
1200 - 1760 °F
Average value: 871 °C Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+10 - 1.00e+16 ohm-cm
1.00e+10 - 1.00e+16 ohm-cm
Average value: 3.26e+14 ohm-cm Grade Count:28
Surface Resistance 1.00e+10 - 1.00e+16 ohm
1.00e+10 - 1.00e+16 ohm
Average value: 4.36e+14 ohm Grade Count:23
Dielectric Strength 18.5 - 45.0 kV/mm
470 - 1140 kV/in
Average value: 27.7 kV/mm Grade Count:23
Dissipation Factor 0.00680 - 0.0200
0.00680 - 0.0200
Average value: 0.0154 Grade Count:3
Comparative Tracking Index 350 - 600 V
350 - 600 V
Average value: 549 V Grade Count:28
Processing Properties Metric English Comments
Processing Temperature 70.0 - 315 °C
158 - 599 °F
Average value: 109 °C Grade Count:6
Nozzle Temperature 271 - 304 °C
520 - 580 °F
Average value: 288 °C Grade Count:3
Die Temperature 310 - 320 °C
590 - 608 °F
Average value: 315 °C Grade Count:6
Melt Temperature 70.0 - 325 °C
158 - 617 °F
Average value: 282 °C Grade Count:14
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Average value: 83.6 °C Grade Count:9
Drying Temperature 70.0 - 85.0 °C
158 - 185 °F
Average value: 77.8 °C Grade Count:14
Moisture Content 0.0500 - 0.200 %
0.0500 - 0.200 %
Average value: 0.171 % Grade Count:12