Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 7014 Performance Paper Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7014 Performance Paper Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmness and strength on a variety of surfaces including high surface energy (HSE) and low surface energy (LSE) plastics, as well as, metals.Information provided by 3M
Physical Properties Metric English Comments
Thickness 22.9 microns
0.900 mil
Adhesive
48.3 microns
1.90 mil
Facestock
63.5 microns
2.50 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.1205 kN/m
0.6875 pli
Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
0.153 kN/m
0.875 pli
LD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.219 kN/m
1.25 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.263 kN/m
1.50 pli
LD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
0.29582 kN/m
1.6875 pli
HD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
0.29582 kN/m
1.6875 pli
HD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.307 kN/m
1.75 pli
HD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.31773 kN/m
1.8125 pli
LD Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.351 kN/m
2.00 pli
HD Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.394 kN/m
2.25 pli
LD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.42729 kN/m
2.4375 pli
Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
0.438 kN/m
2.50 pli
HD Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
0.438 kN/m
2.50 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.44921 kN/m
2.5625 pli
HD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.482 kN/m
2.75 pli
LD Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
0.526 kN/m
3.00 pli
LD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.5916 kN/m
3.375 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
50.0 °C
122 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 320 Acrylic
Liner 43# Densified Kraft
Users viewing this material also viewed the following: