Maximum Service Temperature, Air 200 - 264 °C
392 - 507 °F
Average value: 213 °C Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..