Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 200 - 264 °C | 392 - 507 °F | Average value: 213 °C Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |