Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 141 °C | 286 °F | Long Term |
Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products
(discontinued **) ENSIFONE is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. ENSIFONE is FDA and .. |