Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 - 154 °C
302 - 310 °F
Average value: 150 °C Grade Count:11
Overview of materials for Modified ETFE, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap..