Maximum Service Temperature, Air 193 °C
379 °F
Heat resistance per ASTM D794
Plenco 7300 Phenolic, Nodular, Transfer Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file..
Maximum Service Temperature, Air 193 °C
379 °F
Heat Resistance; ASTM D795
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded  (discontinued **)
This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability ch..
Maximum Service Temperature, Air 193 °C
379 °F
Heat Resistance; ASTM D570D
Plenco 2408 Phenolic, Granular, Compression Molded
PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi..
Maximum Service Temperature, Air 193 °C
379 °F
Heat Resistance; ASTM D570D
Plenco 7200 Phenolic, Granular, Transfer Molded
PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component ..
Maximum Service Temperature, Air 193 °C
379 °F
Short Term
3M 4004 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Maximum Service Temperature, Air 193 °C
379 °F
Short Term
3M 4008 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Maximum Service Temperature, Air 193 °C
379 °F
Short Term
3M 4016 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Maximum Service Temperature, Air 193 °C
379 °F
Short Term
3M 4026 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Maximum Service Temperature, Air 193 °C
379 °F
Short Term
3M 4032 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Maximum Service Temperature, Air 193 °C
379 °F
Short Term
3M 4052 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Maximum Service Temperature, Air 193 °C
379 °F
Short Term
3M 4056 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Maximum Service Temperature, Air 193 °C
379 °F
Short Term
3M 4085 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Maximum Service Temperature, Air 193 °C
379 °F
Heat Resistance; ASTM D570D
Plenco 7307 Phenolic, Granular, Transfer Molded
PLENCO 07307 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties. Type ASTM 5948 CFG, and UL recognized under component file E40654. 07307 is a..